Red Satin Moroccan Sand Glaze
Red Satin is a bright red with a satin surface instead of a glassy one, a touch cooler than a true fire red.
$37.50
Suggested retail price. In-store prices and availability may vary by location.
Laguna's Moroccan Sand glazes fire in oxidation to cone 5/6 in solid, saturated colour. The surface changes with the clay body underneath and with how thickly the glaze is applied. It is brighter over a white body and moves more over porcelain, which pulls more water out of the glaze at the bisque stage. Apply 2 to 3 coats by brush. Lead free and certified non-toxic.
- Cone 5/6 oxidation
- Satin rather than glassy
- 2 to 3 brush coats
- Lead free
- Certified non-toxic to ASTM C-1023 and D-4236