Our email is currently down – please call us if you are trying to get in touch.

Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Laguna  |  MS-54

Emeraude Moroccan Fusion Glaze

Emeraude is a muted mid green with cool blue-grey mottling, breaking cream on raised detail.

$28.15

Suggested retail price. In-store prices and availability may vary by location.

Laguna's Moroccan Fusion glazes fire in oxidation to cone 5/6 in solid, saturated colour. The surface changes with the clay body underneath and with how thickly the glaze is applied. It is brighter over a white body and moves more over porcelain, which pulls more water out of the glaze at the bisque stage. Apply 2 to 3 coats, brushed or dipped. Lead free and certified non-toxic.

  • Cone 5/6 oxidation
  • Glossy, mottled, breaks cream
  • 2 to 3 coats, brushed or dipped
  • Lead free
  • Certified non-toxic to ASTM C-1023 and D-4236