Laguna | MS-49
Oasis Blue Moroccan Fusion Glaze
Oasis Blue is a deep blue-green teal, dark enough that raised detail comes up only a shade lighter.
$28.15
Suggested retail price. In-store prices and availability may vary by location.
Laguna's Moroccan Fusion glazes fire in oxidation to cone 5/6 in solid, saturated colour. The surface changes with the clay body underneath and with how thickly the glaze is applied. It is brighter over a white body and moves more over porcelain, which pulls more water out of the glaze at the bisque stage. Apply 2 to 3 coats, brushed or dipped. Lead free and certified non-toxic.
- Cone 5/6 oxidation
- Glossy, deep and close-toned
- 2 to 3 coats, brushed or dipped
- Lead free
- Certified non-toxic to ASTM C-1023 and D-4236