Laguna | MS-41
Batik Blue Moroccan Sand Glaze
Batik Blue is a warm dark brown, with rust breaking over raised detail and a faint cool grey at the edges.
$28.15
Suggested retail price. In-store prices and availability may vary by location.
Laguna's Moroccan Sand glazes fire in oxidation to cone 5/6 in solid, saturated colour. The surface changes with the clay body underneath and with how thickly the glaze is applied. It is brighter over a white body and moves more over porcelain, which pulls more water out of the glaze at the bisque stage. Apply 2 to 3 coats by brush. Lead free and certified non-toxic.
- Cone 5/6 oxidation
- Glossy, rust break over detail
- 2 to 3 brush coats
- Lead free
- Certified non-toxic to ASTM C-1023 and D-4236