We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

A-4

Kiln Stilt – A-4, 1 1/2 in

A three-point kiln stilt, 38 mm (1 1/2 in) between the metal points, for firing glazed ware clear of the shelf.

$2.59

Suggested retail price. In-store prices and availability may vary by location.

A stilt lifts a fully glazed piece off the kiln shelf on three fine metal points, so glaze on the foot cannot fuse the pot to the shelf. The A-4 spans 38 mm (1 1/2 in) between points. Choose a stilt a little smaller than the foot it carries so the points sit under the base, and grind off the small marks the points leave after firing. Stilts are used mostly for low-fire glazed ware.

  • Stilt A-4
  • 38 mm (1 1/2 in) between points
  • Three metal points
  • Fires glazed feet clear of the shelf
  • Mostly for low-fire ware