Kemper Tools  |  HC1A

HC1A Hole Cutter for Wet Clay

Cuts a clean 6.3 mm (1/4 in) hole in wet clay and thick-walled greenware. 137 mm (5 3/8 in) long overall.

$9.70

Suggested retail price. In-store prices and availability may vary by location.

HC1A cuts a 6.3 mm (1/4 in) hole and is 137 mm (5 3/8 in) long overall. It is made for wet clay and thick-walled greenware, where a drill or a knife would tear the edge. The cutter takes a plug out instead and leaves the rim clean.

  • Kemper HC1A
  • 6.3 mm (1/4 in) cutting diameter
  • 137 mm (5 3/8 in) long overall
  • For wet clay and thick-walled greenware