Plainsman Clays | COPCA
Copper Carbonate
Copper carbonate is the main source of green and turquoise in glazes, and it colours slips as well. It is the more even of the copper additions and disperses without the specking the oxide can give.
$0
Suggested retail price. In-store prices and availability may vary by location.
Copper carbonate is the main source of green and turquoise in glazes. In oxidation it gives green, and in a base high in alkali and low in alumina it gives turquoise. In reduction it is the route to the copper reds such as oxblood and peach bloom, though those need more than a reducing kiln. They need tin in the base, far less copper than a green uses, and a firing that reoxidises at the end. Copper colours slips too, and a slip needs more than a glaze. Copper is a strong flux, so heavy additions run, and past a point the green turns black or metallic. Above about cone 8 some of it evaporates and can leave a blush on nearby pots, which shows most on the tin whites and celadons in the same kiln. It contains less copper per gram than black copper oxide, so seven parts of carbonate stand in for five parts of the oxide.
- The main source of green and turquoise in glazes
- Green in oxidation, turquoise in a high alkali, low alumina base
- The route to copper reds in reduction, with tin in the base
- Disperses evenly, with less specking than black copper oxide
- Seven parts stand in for five parts of black copper oxide
- A strong flux, heavy additions run and the green turns black
- Evaporates above about cone 8 and can blush tin glazes in the same kiln