Colorobbia | 10057899
Colorobbia Iris Lustre
A mother of pearl overglaze lustre that fires to a thin, iridescent rainbow sheen over glazed ware.
$29.65
Suggested retail price. In-store prices and availability may vary by location.
Brush it over a glaze that has already been fired, then fire again at a low temperature. It goes on as a dark liquid and fires to a clear, shimmering film that takes on the colour of the glaze beneath, with the most sparkle over glossy glaze. Brush a thin, even coat onto a clean, dry surface, and thin it with Colorobbia lustre thinner if it drags. Fire with the kiln well vented, and work in a well ventilated room with the lustre kept off your skin.
- Mother of pearl iridescent finish
- Goes over fired glaze
- Cone 019 to 018, about 720 to 750°C (1330 to 1385°F)