Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  949P

949 Deep Sea Low Stone Glaze

A mid teal blue, mottled darker in bands.

$39.50

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 900 series is a low fire glaze with the look of stoneware, and the colours can be layered over one another for more effects. The surface is semi-gloss and speckled. Three coats on white bisque give the full colour. Spectrum rates the series cone 06 to 04, 1015 to 1060°C, with cone 05 the recommended firing. Do not use it on the same piece as a 700 series glaze, because the two expand at different rates and the combination can crack. Lead-free. Spectrum does not rate it non-toxic in the liquid state.

  • Cone 06 to 04, 1015 to 1060°C
  • A mid teal blue, mottled darker in bands
  • Semi-gloss speckled surface
  • Not for use with a 700 series glaze on the same piece
  • Lead-free
  • Not rated non-toxic in the liquid state