Spectrum  |  935P

935 Purple Haze Low Stone Glaze

A bright lilac purple with dark speckle.

$26

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 900 series is a low fire glaze with the look of stoneware, and the colours can be layered over one another for more effects. The surface is semi-gloss and speckled. Three coats on white bisque give the full colour. Spectrum rates the series cone 06 to 04, 1015 to 1060°C, with cone 05 the recommended firing. Do not use it on the same piece as a 700 series glaze, because the two expand at different rates and the combination can crack. Lead-free and AP non-toxic. Conforms to ASTM D-4236.

  • Cone 06 to 04, 1015 to 1060°C
  • A bright lilac purple with dark speckle
  • Semi-gloss speckled surface
  • Not for use with a 700 series glaze on the same piece
  • Lead-free and AP non-toxic
  • Conforms to ASTM D-4236