Spectrum  |  932P

932 Pistachio Low Stone Glaze

A bright light green, heavily flecked with black.

$29

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 900 series is a low fire glaze with the look of stoneware, and the colours can be layered over one another for more effects. The surface is semi-gloss and speckled. Three coats on white bisque give the full colour. Spectrum rates the series cone 06 to 04, 1015 to 1060°C, with cone 05 the recommended firing. Do not use it on the same piece as a 700 series glaze, because the two expand at different rates and the combination can crack. Lead-free.

  • Cone 06 to 04, 1015 to 1060°C
  • A bright light green, heavily flecked with black
  • Semi-gloss speckled surface
  • Not for use with a 700 series glaze on the same piece