Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  931P

931 Dove Gray Low Stone Glaze

A soft blue grey with dark brown speckle.

$34

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 900 series is a low fire glaze with the look of stoneware, and the colours can be layered over one another for more effects. The surface is satin and speckled. Three coats on white bisque give the full colour. Spectrum rates the series cone 06 to 04, 1015 to 1060°C, with cone 05 the recommended firing. Do not use it on the same piece as a 700 series glaze, because the two expand at different rates and the combination can crack. Lead-free and AP non-toxic. Conforms to ASTM D-4236.

  • Cone 06 to 04, 1015 to 1060°C
  • A soft blue grey with dark brown speckle
  • Satin speckled surface
  • Not for use with a 700 series glaze on the same piece
  • Lead-free and AP non-toxic
  • Conforms to ASTM D-4236