906 Burnt Sugar Low Stone Glaze

A warm amber gold banded with dark rust brown.

$32

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 900 series is a low fire glaze with the look of stoneware, and the colours can be layered over one another for more effects. The surface is a glossy semi-transparent two-tone. Three coats on white bisque give the full colour. Spectrum rates the series cone 06 to 04, 1015 to 1060°C, with cone 05 the recommended firing. Do not use it on the same piece as a 700 series glaze, because the two expand at different rates and the combination can crack. Lead-free.

  • Cone 06 to 04, 1015 to 1060°C
  • A warm amber gold banded with dark rust brown
  • Glossy semi-transparent two-tone
  • Not for use with a 700 series glaze on the same piece
  • Lead-free