Spectrum  |  743P

743 Bright Red Opaque Gloss Glaze

A strong clear red with a slight orange lean, opaque and very glossy.

$20

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 700 series is a low fire gloss glaze with solid, opaque colour, so the clay underneath does not show through. Two to three brush coats give full coverage. These colours do not tend to bleed, so one can be painted right up against another. Spectrum rates the series cone 06 to 04, 1015 to 1060°C. Lead-free and AP non-toxic. Conforms to ASTM D-4236. Contains an encapsulated cadmium pigment.

  • Cone 06 to 04, 1015 to 1060°C
  • A strong clear red with a slight orange lean, opaque and very glossy
  • Opaque coverage in 2 to 3 brush coats
  • Does not tend to bleed, colours can sit edge to edge
  • Lead-free and AP non-toxic, contains encapsulated cadmium pigment
  • Conforms to ASTM D-4236