Amaco | V-354
V-354 Leaf Green Velvet Underglaze
A soft, bright jade green at cone 05.
$45.50
Suggested retail price. In-store prices and availability may vary by location.
It darkens to a deep blue green at cone 5 and a dark forest green at cone 10. A clear glaze over it intensifies the colour at any temperature. Velvet is AMACO's underglaze line. It is opaque, matches the colour in the jar and is fine enough to hold detailed brushwork. Brush it on wet clay, leather hard clay, greenware or cone 04 bisque, whichever stage suits the piece. It fires anywhere from cone 05 to cone 10, and left bare it dries to the soft matte finish it is named for. Three to four brush coats give full coverage, and it can also be sprayed or layered. On its own it is not food safe, but it becomes dinnerware safe once a food safe clear glaze is fired over it. Fire a test tile with each new batch.
- Cone 05 to 10 underglaze
- Soft jade green, deeper at higher cones
- Intensifies under a clear glaze
- Brush on wet clay, greenware or cone 04 bisque
- 3 to 4 coats, can be sprayed or layered
- Dinnerware safe under a food safe clear glaze
- AP non toxic, conforms to ASTM D-4236