Proudly Canadian

We are a Canadian company, based in Southern Alberta, serving the pottery industry since 1966.

Spectrum  |  263P

263 Satin Quebec Blue Glaze

A cornflower blue that pales over raised edges.

$22

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 250 series is a cone 06/04 low fire opaque glaze with a satin surface. Two to three brush coats give solid coverage. It is a stiff glaze that moves very little in the firing, so an even application matters more than it would with a gloss. It also responds to temperature, and the hotter it is fired within the range the smoother and glossier the surface comes out. Spectrum rates the series cone 06 to 04, 1015 to 1060°C. Lead-free and AP non-toxic. Dinnerware safe.

  • Cone 06 to 04, 1015 to 1060°C
  • A cornflower blue that pales over raised edges
  • Opaque satin surface
  • 2 to 3 brush coats
  • Stiff glaze, apply evenly
  • Glossier at the hot end of the range
  • Lead-free and AP non-toxic
  • Dinnerware safe