155 Brushed Bronze Low Fire Metallic Glaze

A mottled bronze that shifts between gold, mauve, and green across one surface.

$44

Suggested retail price. In-store prices and availability may vary by location.

Spectrum's 150 series fires to a metallic surface. This colour has a matte finish. It needs an accurate cone 05 firing, around 1030°C, and a heavy coat, three generous brush coats or four normal ones. Fire it to cone 05 exactly. Cone 06 is too cool and cone 04 too hot, and a thin or underfired coat comes out a dull matte black or green. Iron or manganese in the clay body can affect the finish, and so can a slow cool or a tightly packed kiln, which grow crystals that dull the metal. Bisque fired in the same load gives off gases that affect the surface too. It is lead-free but not dinnerware safe.

  • Cone 05 only, about 1030°C
  • A mottled bronze that shifts between gold, mauve and green across one surface
  • Matte metallic finish
  • Heavy application, 3 generous brush coats or 4 normal
  • Too hot, too cool or too thin fires a drab black or green
  • Lead-free
  • Not dinnerware safe