Spectrum | 1472P
1472 Watermelon Semi-Transparent Glaze
A clean bright red.
$14.50
Suggested retail price. In-store prices and availability may vary by location.
Spectrum's 1460 series is a cone 4/6 stoneware glaze with a semi-transparent high gloss surface. It darkens where it pools in carved and impressed detail and stays clear enough to show an underglaze design through it. Three brush coats on low-fired bisque give the full colour. Spectrum rates the series cone 4 to 6, 1190 to 1230°C. Lead-free.
- Cone 4 to 6, 1190 to 1230°C
- A clean bright red
- Semi-transparent high gloss, darkens where it pools
- Three brush coats
- Lead-free