Spectrum | 1138P
1138 Lime Green Stoneware Glaze
A bright yellow green.
$16
Suggested retail price. In-store prices and availability may vary by location.
This is one of Spectrum's 1100 series stoneware glazes. It fires to an opaque gloss, so the clay body will not show through, and it is brighter over a white body than a dark one. Brush on three coats for full colour and fire to cone 5, which is where it will match the jar. It will fire anywhere from cone 4 to cone 6, 1190 to 1230°C, but expect the colour to shift a little at either end. Lead free and AP non toxic. Conforms to ASTM D-4236.
- Cone 4 to 6, cone 5 recommended
- A bright yellow green
- Opaque gloss
- Three brush coats
- Lead free and AP non toxic
- Conforms to ASTM D-4236